CalcWorldHub
Free online calculator · no signup

Brinell Hardness Calculator

Calculate Brinell hardness from a ball indenter diameter, applied force, and measured impression diameters.

4,000 tools
Brinell Hardness Calculator — Test force (kgf), Ball diameter, D (mm), Impression diameter d₁ (mm) and calculation method
Brinell Hardness Calculator: inputs and calculation method.

How to use this calculator

Calculate Brinell hardness from a ball indenter diameter, applied force, and measured impression diameters.

  1. Enter Test force (kgf), Ball diameter, D (mm), Impression diameter d₁ (mm), Perpendicular impression diameter d₂ (mm). Match the units shown beside each field and review the result together with the assumptions below.
  2. Read the worked example below to check the expected input format and result.
  3. Compare another scenario by changing one input at a time. Use Reset to return to the starting values.
Manufacturing calculation

How this calculation works

The Brinell test relates the applied force to the curved surface area of the spherical indentation. Two perpendicular impression diameters can be averaged to reduce simple measurement-direction variation before calculating the hardness number.

Inputs and units

forceKgf — Test force (kgf)
Applied Brinell test force in kilogram-force.
ballDiameterMm — Ball diameter, D (mm)
Diameter of the spherical tungsten-carbide ball.
impressionD1Mm — Impression diameter d₁ (mm)
First measured impression diameter.
impressionD2Mm — Perpendicular impression diameter d₂ (mm)
Second impression diameter measured perpendicular to d₁.

Formula

Displayed formula

HBW = 2F/[πD(D − √(D² − d²))], where d = (d₁ + d₂)/2 and F is in kgf.

Method

Enter test force in kgf, tungsten-carbide ball diameter D in mm, and two perpendicular impression diameters d₁ and d₂ in mm. The calculation uses their mean and requires each impression diameter to be smaller than the ball diameter.

Worked example

For a 3000 kgf force, a 10 mm ball, and perpendicular impression diameters of 4.5 mm and 4.7 mm, the mean diameter is 4.60 mm and the calculated hardness is 170.40 HBW.

Assumptions and limits

Use the force, indenter, dwell time, surface preparation, and measurement procedure required by the applicable test standard. This formula does not determine whether a test setup or result conforms to a material-specific standard.

Frequently asked questions

Why enter two impression diameters?

The measured impression can be slightly noncircular, so two perpendicular diameters are averaged in this calculator.

What does HBW mean?

It denotes a Brinell hardness test using a tungsten-carbide ball indenter.

Does this check standard compliance?

No. Compliance also depends on the specified force, ball, dwell, specimen, and test procedure.

How do I use the Brinell Hardness Calculator?

Enter Test force (kgf), Ball diameter, D (mm), Impression diameter d₁ (mm), Perpendicular impression diameter d₂ (mm). Match the units shown beside each field and review the result together with the assumptions below.

What is a worked example of Brinell Hardness?

For a 3000 kgf force, a 10 mm ball, and perpendicular impression diameters of 4.5 mm and 4.7 mm, the mean diameter is 4.60 mm and the calculated hardness is 170.40 HBW.